Type 4 CoCr metal-ceramic alloy – Co 60,0 %, Cr 24,5 %, W 9,0 %, Nb 2,0 %, V 2,0 %, Mo 1,1 %. For ceramic-veneered crowns and bridges, telescopic c...

Watch this product and we will notify you once it is back in stock.

The product is now watched
We will notify you once the product is back in stock again.

KeraGen CoCr, type 4, 1000 g

Type 4 CoCr metal-ceramic alloy – Co 60,0 %, Cr 24,5 %, W 9,0 %, Nb 2,0 %, V 2,0 %, Mo 1,1 %. For ceramic-veneered crowns and bridges, telescopic c...

Description

Type 4 CoCr metal-ceramic alloy for dental laboratory use. The product is intended for the specific casting, welding, soldering or titanium application stated by the manufacturer.

Product facts

  • Type: Type 4 CoCr metal-ceramic alloy
  • Metal composition: Co 60,0 %, Cr 24,5 %, W 9,0 %, Nb 2,0 %, V 2,0 %, Mo 1,1 %; Si/Fe ≤ 1,0 %

Technical data

Eisenbacher specifies type 4, 350 HV, density 8.4 g/cm³ and recommended casting temperature 1485 °C.

Applications

For ceramic-veneered crowns and bridges, telescopic crowns, combination and attachment work.

Reviews

Product review Based on 0 ratings.

Click on a star to rate
You
Retrieve your Facebook profile.
  • Be the first to leave a review.

Free delivery on orders over 500 €

Secure and fast delivery

Pay on delivery by invoice

JavaScript seem to be disabled in your browser.

You must have JavaScript enabled in your browser to utilize the functionality of this website.